My name is Frank and I am graduate student new to using the Comsol software. I am currently having issues increasing the cycle number from 2000 cycles up to 4000 cycles for capacity fade of a Lithium ion battery, and would love to find any assistance at all I can get.
I am currently running a capacity fade simulation for 2000 cycles and have obtained my initial results.
I tried increasing the cycle number from 2000 cycles to 4000 cycles by editing the capacity fade parameter and changing the no of cycles from 2000 cycles to 4000 cycles, having a closer look at my graph for this number of cycles, I noticed an error in the result, the Relative capacity does not start from an initial 1C, but starts from 0.86C which cannot be correct.
Please find attached a comparison of my results for 2000 cycles and 4000 cycles.
Attachments:
- 1SEI layer Potential drop (4000 cycles).png
 - Capacity vs Cycle number (4000 cycles).png
 - Capacity vs Time (4000 cycles).png
 - Electrolyte volume fraction (4000 cycles).png
 - SEI layer Potential drop at 1C (2000 cycels).png
 - Capacity vs cycle number (2000 cycles).png
 - Capacity vs Time (2000 cycles).png
 - Electrolyte Volume Fraction (2000 cycles).png
 
Hello Frank Ajieh
Your Discussion has gone 30 days without a reply. If you still need help with COMSOL and have an on-subscription license, please visit our Support Center for help.
If you do not hold an on-subscription license, you may find an answer in another Discussion or in the Knowledge Base.