铜集流体溶解
Application ID: 126981
The copper current collector on negative graphite electrodes in lithium-ion batteries have been seen to dissolve at over discharge. This can be a safety concern as the dissolution damages the current collector irreversibly and dissolved copper ions can redeposit and form dendrites. Batteries are usually operated within specified voltage limits, either on cell or pack level, in order to avoid over discharge. However, over discharge may still occur, either in a pack due to charge imbalances between the individual cells, or, as we will partly investigate in this tutorial, due to local heterogeneities in the electrodes within a single battery cell.
This tutorial investigates the copper current-collector dissolution during overdischarge from an electrode with an inhomogeneous graphite electrode material coating thickness. The cuprous ion concentration, as well as the redeposited copper distribution in the cell, are predicted.
案例中展示的此类问题通常可通过以下产品建模:
您可能需要以下相关模块才能创建并运行这个模型,包括:
建模所需的 COMSOL® 产品组合取决于多种因素,包括边界条件、材料属性、物理场接口及零件库,等等。不同模块可能具有相同的特定功能,详情可以查阅技术规格表,推荐您通过免费的试用许可证来确定满足您的建模需求的正确产品组合。如有任何疑问,欢迎咨询 COMSOL 销售和技术支持团队,我们会为您提供满意的答复。